A study of natural pigment-based colour masterbatches has found that four commercial bio-based colorants can be compounded into polylactic acid (PLA) and polybutylene succinate (PBS) on conventional twin-screw extrusion and injection moulding equipment, with only modest changes to melt flow and mechanical performance. The main obstacle identified is not processing but lightfastness.
The work, published under the title "Sustainability in the Development of Natural Pigment-Based Colour Masterbatches and Their Application in Biopolymers," examined blue spirulina, yellow curcumin, red beetroot and green chlorophyllin. Each pigment was combined with PLA and with PBS to produce colour masterbatches, which were then let down into the matching polymer matrix at 2, 4 and 6 wt% and injection moulded into test specimens. The masterbatch formulation also contained titanium dioxide, calcium carbonate and stearic acid, added to support UV protection, pigment dispersion and processing.
Heat set the tightest constraint. Thermogravimetric analysis put the degradation onset at approximately 229 °C for spirulina, 244 °C for curcumin, 258 °C for chlorophyllin and 267 °C for beetroot, below the degradation temperatures measured for PLA and PBS. The researchers therefore selected extrusion profiles that melted each polymer while limiting the pigments' thermal exposure, reaching 145 °C for PBS and 190 °C for PLA. The twin-screw extruder ran at 65 rpm with a feed rate of 2 kg/h.
That window suited most pigment–polymer pairs, with one exception. During PLA processing, spirulina lost its characteristic blue colour, so no blue PLA masterbatch could be produced. In PBS, whose lower processing temperature limited the thermal load, the same pigment retained enough stability to be compounded successfully. The study presents the result as evidence that pigment compatibility depends strongly on the thermal requirements of the polymer matrix, not on the colorant alone.
Rheology moved little. Melt flow rate fell slightly after pigment incorporation, indicating a modest rise in melt viscosity. Neat PLA measured about 50 g/10 min, and the natural-pigment masterbatches stayed close to that figure; PBS responded similarly, with only a minor reduction. For compounders the point is practical: a colour system that forces changes to screw design, pressure settings or moulding conditions would offer limited value, and most formulations here ran on standard equipment without major processing problems.
Mechanical testing covered the same 2 to 6 wt% addition range. PLA started at a Young's modulus of about 1710 MPa and a tensile strength of 65.6 MPa; PBS started at about 392 MPa and 34.5 MPa respectively. The coloured formulations stayed close to those baselines, and impact strength remained within a similar range, although individual pigments produced some variation.
Durability proved harder to hold. After 50 hours of xenon-lamp exposure, most formulations showed a colour difference above ΔE* = 2, the level generally taken to mark a visually perceptible change. The clearest exception was a PLA formulation containing 2 wt% green chlorophyllin masterbatch, which showed the highest photostability in the set. The study consequently identifies UV stability as the largest barrier to broader use, noting that packaging, consumer products, agricultural parts and outdoor applications may require additional stabilisation, protective coatings or pigment modification before natural colours can compete with conventional systems over long service periods.
Successful extrusion did not guarantee long-term colour retention, and the researchers separate the two questions: several colorants can be processed, but their stability in service remains unresolved.
The environmental comparison favoured the natural route under the study's assumptions. One kilogram of curcumin pigment was associated with about 0.04 kg CO2-eq, against 18.65 kg CO2-eq for the inorganic green reference pigment, and the natural-pigment masterbatches also consumed less electricity during extrusion and pelletising.
The authors conclude that natural pigment masterbatches still require development in lightfastness and thermal stability, but that several colorants can be compounded into PLA and PBS on conventional equipment with limited penalty in melt viscosity and mechanical performance. Future work, they suggest, should focus on improving colour stability both during processing and in subsequent service exposure.